LMP-based Creep Rupture Estimate of an Alloy 617 Serpentine Superheater Tube Using Ansys

G. Aravindhan, P.P. Shantharaman

👁 1 view📥 0 downloads
Share: 𝕏 f in ✈ ✉
Abstract: Superheater tubes in ultra-supercritical power plants operate at high temperatures and pressures for prolonged periods, making creep rupture an important life-limiting mechanism. This study investigates the thermal-structural behaviour and estimates the creep-rupture life of an Alloy 617 serpentine superheater tube using finite element analysis and the Larson–Miller parameter method. The tube (OD 50.8 mm, ID 37.1 mm) carries steam at 700 °C and 300 bar and is heated externally by flue gas at 1500 K. The maximum wall temperature predicted by ANSYS is 733.84 °C. The computed temperatures agree with published straight-tube results within 0.5%. The inner-wall maximum principal stress of 96.08 MPa agrees with the Lamé thick-wall hoop stress of 98.6 MPa within 2.6%. Changing the mesh size from 4.5 mm to 5 mm alters the maximum stress by only 0.05%, although this does not establish mesh convergence. The bend peak von Mises stress reaches 143.47 MPa, approximately 1.3 times the straight-section inner-wall value of 108.65 MPa. The estimated rupture life is approximately 24,000 h without the standard-error correction and 6,600 h with it at the analytical hoop stress, decreasing to about 2,300 h at the bend peak stress. These estimates are below the 100,000 h design-life target discussed in the reference study. The findings highlight the influence of bend-induced stress concentration and stress selection on predicted rupture life. The results provide a preliminary estimate of creep-rupture life, and further validation is required.

Keywords: Alloy 617; superheater tube; Larson-Miller parameter; creep rupture; finite element analysis