📞 +91-7667918914 | ✉️ iarjset@gmail.com
International Advanced Research Journal in Science, Engineering and Technology
International Advanced Research Journal in Science, Engineering and Technology A Monthly Peer-Reviewed Multidisciplinary Journal
ISSN Online 2393-8021ISSN Print 2394-1588Since 2014
IARJSET aligns to the suggestive parameters by the latest University Grants Commission (UGC) for peer-reviewed journals, committed to promoting research excellence, ethical publishing practices, and a global scholarly impact.
← Back to VOLUME 2, ISSUE 6, JUNE 2015

RESEARCH ON SUCTION CASTING DEFECTS OF AL BASED ALLOY LINKAGE

Wang Zexuan, He Tao, Yang Yong, Li Yan

👁 34 views📥 0 downloads
Share: 𝕏 f in ✈ ✉

Abstract: The filling process and solidification of Al based alloy linkage by suction casting was studied via numerical simulation. The shrinkage defect of Al based alloy linkage casting was predicted by using FEM software ProCAST. The results indicate the cold shut will be decreased with the increase of graphite suction opening diameter and the pouring temperature. With the decrease of the coefficient of heat transfer, the cold shut is reduced. The Al based alloy linkage are obtained by this method. The simulated result tallies well with the actual cast experiment, and lays down a foundation for improving the cast technology of the Al based alloy casting.

Keywords: FEM simulation; ProCAST software; suction casting; shrinkage defect.

How to Cite:

[1] Wang Zexuan, He Tao, Yang Yong, Li Yan, “RESEARCH ON SUCTION CASTING DEFECTS OF AL BASED ALLOY LINKAGE,” International Advanced Research Journal in Science, Engineering and Technology (IARJSET), DOI: 10.17148/IARJSET.2015.2601

Creative Commons License This work is licensed under a Creative Commons Attribution 4.0 International License.